Wayar ribbon mai amfani da hasken rana don samar da wutar lantarki mai inganci
Bayani
Dongke Solar RIBBON wani nau'in waya ce mai ƙarfi da carbon mai ƙarfi, mai tauri sosai, kuma mai juriyar lalacewa. Ana amfani da ita a matsayin mai ɗaukar kayan yanka waya da yawa don yanke kayan lu'ulu'u masu ƙarfi, kamar silicon, gallium arsenide, indium phosphide, silicon carbide da lu'ulu'u.
Fa'idodin samfur
Rage asarar kerf;
Ingantaccen aiki, iya aiki da daidaito;
Ƙarancin kuɗin sarrafawa.
Fa'idodin Marsrock
Samun kayan aiki masu inganci da muhimman abubuwan amfani a duniya;
Injin samarwa na ajin farko da ingantaccen tsari;
Ƙungiyar ƙwararru masu ƙwarewa a fannin samarwa da fasaha;
Kayan aikin dakin gwaje-gwaje mafi ci gaba;
. Ƙwarewar bincike da ci gaba mai kyau, tana bayar da samfuran da aka keɓance;
ISO9001: 2008 an tabbatar da shi;
. Faɗaɗɗen ayyuka da ayyukan fasaha.
ƙayyadaddun bayanai
| 1. Sigar Tagulla ta Tushe | |
| Alamar kasuwanci ta tagulla ta tushe | Tagulla C1022 mara iskar oxygen |
| Tsarkakakkiyar jan ƙarfe | Cu≥99.97% |
| Maida wutar lantarki | ≥100% IACS |
| Juriya | ≤0.01724 Ω·m m2/m |
| 2. Kauri da Tsarin Rufi (ana iya keɓance shi bisa ga buƙatun fasaha na abokan ciniki) | |||
| Nau'in Alloy Mai Shafi | Tsarin Shafi | Kauri na Rufi (mm) | Juriyar Kauri Mai Rufi (mm) |
| Jagora | Sn60% Pb40% | 0.01-0.04 | ±0.01 |
| Sn62% Pb36% Ag2% | 0.01-0.04 | ±0.01 | |
| babu gubar | Sn97% Ag3% | 0.01-0.04 | ±0.01 |
| 3. Halayen Inji don Samfurin Commen Spool | |
| Ƙarawa | ≥15% |
| Ƙarfin tauri | ≥150MPa |
| Side camber | L≤8mm/1000mm |
| 4. Girman Jiki da Juriyar Samfurin Spool Na Gama-gari | |||
| Nisa mai kauri | 0.045-0.35mm (ana iya keɓancewa bisa ga buƙatun fasaha na abokan ciniki) | ||
| Juriyar kauri | ±0.02mm | ||
| Faɗin faɗi | 1.0-2.5mm (ana iya keɓancewa bisa ga buƙatun fasaha na abokan ciniki) | ||
| Juriyar faɗi | ±0.08mm | ||
| Bayani na Musamman na Tabbing Ribbon (mm) (Spool Package) | |||
| 0.18 × 2.0 | 0.22×2.0 | 0.24×2.0 | 0.27 × 2.0 |
| 0.20 × 1.5 | 0.23×1.5 | 0.25×1.5 | 0.30 × 1.5 |
| 0.20 × 1.6 | 0.23×1.6 | 0.25×1.6 | 0.30 × 1.6 |
| 0.2 × 1.8 | 0.23×1.8 | 0.25×1.8 | 0.30 × 1.8 |
| 0.2 × 2.0 | 0.23×2.0 | 0.25×2.0 | 0.30 × 2.0 |
Yanayin Ajiya da Tsawon Lokacin Shiryawa
Ya kamata a adana kintinkirin tagulla da aka yi da gwangwani a cikin ɗaki busasshe kuma mai iska, inda bai kamata a sami sinadarin acid, alkail, ko iskar gas mai cutarwa ba, kuma danshi na cikin gida bai kamata ya wuce kashi 60% ba, a ajiye shi a kwance yayin da ake tara shi, a guji fitar da kwalin da kuma sanya shi a tsaye, yayin da adadin samfuran iri ɗaya bai wuce layuka biyar ko tan 1 ba. Tsawon lokacin shiryawa zai iya kaiwa har zuwa watanni shida tun daga ranar da aka samar.